13 Clay

Alternate Names: #13 Clay

Description: Plastic Clay - Allier, France

Oxide Analysis Formula Tolerance
CaO 0.30% 0.02
K2O 1.80% 0.07
MgO 0.40% 0.03
Na2O 0.10% 0.01
TiO2 1.40% 0.06
Al2O3 29.50% 1.00
SiO2 53.60% 3.08
Fe2O3 3.30% 0.07
LOI 9.60%n/a
C 0.20%n/a
Oxide Weight 312.57
Formula Weight 346.53

Related Information

Links

Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.