Silica Yuba

Description: GROUND SILICA FLOUR

Oxide Analysis Formula Tolerance
K2O 0.01% 0.18
Al2O3 0.06% 1.00
SiO2 99.86%
Fe2O3 0.02% 0.21
LOI 0.05%n/a
Oxide Weight 169,915.00
Formula Weight 170,000.00

Notes

Sieve analysis: YubaSil 140# 200# 200F# 300# 325# 325P
------------------------------------------------
Retain on US 60 t
80 t t
100 t t t t t
140 15 5 1 1 t t
200 28 8 4 2 2 t t
270 17 9 4 7 3 1 1
325 23 11 14 8 4 4 2

Bulking Value, gals/lb: .046
Apparent Density (dry uncompacted) 90.6 lbs/cubic foot
pH (37.5% suspension): 6.5
Oil Absorption ASTM D-1483: 20 lbs/100 lbs pigment
Specific Surface Area: 1.05 square meters per gram
G.E. Brightness: 86-88
Specific Gravity: 2.65
Porosity: Non-porous

Related Information

Links

Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.