Shiro Sekkai Whiting

Oxide Analysis Formula Tolerance
CaO 55.17% 0.99
K2O 0.98% 0.01
Al2O3 0.62% 0.01
SiO2 0.11% -
Fe2O3 0.11% -
LOI 43.01%n/a
Oxide Weight 57.34
Formula Weight 100.62