Red Mesa Fireclay

Alternate Names: Red Mesa Clay, Vista Red

Oxide Analysis Formula Tolerance
SiO2 54.50% 5.23
Al2O3 17.70% 1.00
Na2O 2.02% 0.19
Fe2O3 8.04% 0.29
CaO 0.10% 0.01
MgO 0.86% 0.12
K2O 1.41% 0.09
LOI 9.04%n/a
Oxide Weight 487.70
Formula Weight 536.17

Related Information

Links

Materials Fireclay
Typecodes Fireclay
Fireclays are non-kaolin non-ball clay materials similar to stoneware clays but lacking fluxing oxides. Many fireclays have a PCE of 28 or more.

Data

Frit Softening Point 3000F