1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

RCG-6000

Oxide Analysis Formula Tolerance
CaO 6.71% 0.50
K2O 0.40% 0.02
Na2O 5.56% 0.38
ZnO 1.91% 0.10
ZrO2 9.74% 0.33
B2O3 14.42% 0.87
Al2O3 6.97% 0.29
SiO2 54.29% 3.81
Oxide Weight 421.87
Formula Weight 421.87