RCG-3065

Oxide Analysis Formula Tolerance
CaO 12.54% 0.65
K2O 1.24% 0.04
Li2O 0.49% 0.05
MgO 0.80% 0.06
Na2O 4.28% 0.20
ZrO2 0.41% 0.01
B2O3 6.41% 0.27
Al2O3 10.40% 0.30
SiO2 63.44% 3.09
Oxide Weight 292.36