Potassium Dichromate

Description: A bright red-orange crystalline powder

Oxide Analysis Formula Tolerance
K2O 32.02% 1.00
Cr2O3 67.98% 1.32
Oxide Weight 294.19
Formula Weight 294.19

Related Information

Links

Materials Potassium Chromate
Hazards Chromium Compounds Toxicology
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.
URLs http://en.wikipedia.org/wiki/Potassium_dichromate
Potassium Dichromate at Wikipedia
URLs http://www.ilo.org/public/english/protection/safework/cis/products/icsc/dtasht/_icsc13/icsc1371.htm
Potassium Dichromate at ilo.og
Oxides Cr2O3 - Chrome Oxide