PBX Valentine

Oxide Analysis Formula Tolerance
CaO 0.02% -
K2O 0.11% -
MgO 0.23% 0.02
Na2O 0.03% -
TiO2 1.70% 0.07
Al2O3 31.01% 1.00
SiO2 45.56% 2.49
Fe2O3 6.08% 0.12
LOI 15.25%n/a
Oxide Weight 278.73
Formula Weight 328.89