Oxford Feldspar

Description: Potash Feldspar

Oxide Analysis Formula Tolerance
CaO 0.39% 0.05
K2O 8.07% 0.59
Na2O 3.28% 0.36
Al2O3 17.35% 1.17
SiO2 70.82% 8.10
Fe2O3 0.09% -
LOI 0.18%n/a
Oxide Weight 687.17
Formula Weight 688.41

Notes

This material is no longer available. In determining a substutite considering the proportion of K2O to Na2O in the formula is helpful.
Eureka #703, Kona A-3 or Custer feldspar are a good substitutes.

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy