1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Odo

Oxide Analysis Formula Tolerance
CaO 0.35% 0.04
K2O 2.18% 0.14
MgO 0.71% 0.11
Na2O 0.55% 0.05
TiO2 0.96% 0.07
Al2O3 16.70% 1.00
SiO2 62.59% 6.36
Fe2O3 8.71% 0.33
LOI 7.25%n/a
Oxide Weight 566.50
Formula Weight 610.78