Ochre

Oxide Analysis Formula Tolerance
CaO 0.50% 0.15
MgO 0.20% 0.08
Al2O3 6.03% 1.00
SiO2 25.11% 7.07
Fe2O3 55.65% 5.89
MnO 3.01% 0.72
LOI 9.50%n/a
Oxide Weight 1,531.61
Formula Weight 1,692.38

Notes

A very high-iron clay-like material available in many parts of the world. The iron concentration (coupled with manganese which is often present) makes it a powerful colorant for bodies, engobes, underglazes, and overglaze decoration (tan, brown, grey, black and brick red hues).

Related Information

Links

Materials Ochre
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy