Nezumi Sekkai Whiting

Oxide Analysis Formula Tolerance
CaO 54.50% 319.65
K2O 0.02% 0.07
MgO 0.06% 0.49
Na2O 0.21% 1.11
Al2O3 0.31% 1.00
SiO2 0.46% 2.52
Fe2O3 0.05% 0.10
LOI 44.39%n/a
Oxide Weight 18,297.48
Formula Weight 32,903.23