Nan Kang Stone

Oxide Analysis Formula Tolerance
CaO 0.28% 0.03
K2O 3.30% 0.22
MgO 0.60% 0.09
Na2O 1.97% 0.20
TiO2 0.05% -
Al2O3 16.03% 1.00
SiO2 75.14% 7.96
Fe2O3 0.42% 0.02
LOI 2.21%n/a
Oxide Weight 622.24
Formula Weight 636.31