Bentolite H

Description: White processed bentonite

Oxide Analysis Formula Tolerance
K2O 0.10% 0.01
Al2O3 13.50% 0.91
Na2O 3.50% 0.39
TiO2 0.20% 0.02
SiO2 68.10% 7.79
Fe2O3 0.70% 0.03
MgO 2.90% 0.49
CaO 0.90% 0.11
LOI 9.10%n/a
Oxide Weight 617.80
Formula Weight 679.65

Notes

Bentolite H is a white bentonite with a small particle size and high surface area and is popular in oil absorbing applications (e.g. medicated soap bars). It can act as a rheological aid in water based systems imparting thixotropic flow properties.

In glazes, when used in combination with carboxymethylcellulose, Bentolite provides for improved rheology, solids suspension, glaze adhesion, sprayability, and acceptance rates.

Was made by Southern Clay products but discontinued by new owners.

Related Information

Links

URLs http://www.gelwhite.com/tb/tb2.html
TB2 Data Sheet
Materials Laponite RD
Materials BENTOLITE L10
Materials Bentolite L-3
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.