Monthly Tech-Tip from Tony Hansen SignUp

No tracking! No ads!

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Beni Feldspar

Oxide Analysis Formula Tolerance
CaO 0.16% 0.02
K2O 11.64% 0.67
MgO 0.07% 0.01
Na2O 2.69% 0.24
TiO2 0.01% -
Al2O3 18.69% 1.00
P2O5 0.01% -
SiO2 66.59% 6.05
Fe2O3 0.02% -
LOI 0.12%n/a
Oxide Weight 545.09
Formula Weight 545.75

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.