Zochem Grade 500 Zinc Oxide

Oxide Analysis Formula Tolerance
PbO 0.05% -
ZnO 99.70% 1.00
LOI 0.30%n/a
Oxide Weight 81.43
Formula Weight 81.67

Notes

Their general purpose product, recommended for ceramics. Their data sheet states:

Grade 500 is a brilliant white powder manufactured by the French (Indirect) Process. Grade 500 is a popular general use high quality lower lead (Pb) zinc oxide. It meets GMP 21CFR110, is USFDA approved as GRAS (Generally Recognized As Safe) at 21cfr182.8991 and is authorized by the USFDA for use wherever GRAS is approved including food contact in rubber, plastics, and coatings. Grade 500 also meets the requirements of ASTM specification D79, 2000/53/EC End of Life Vehicles (ELV Directive), 2002/95/EC Restriction of Hazardous Substances Directive (RoHS) for heavy metals and Waste Electrical and Electronic Directive (WEEE), and other regulations where high quality zinc oxide is required.

The iron content is so low that we have not quoted it.

Related Information

Links

URLs https://www.zochem.com/wp-content/uploads/2018/04/Grade-500.pdf
Zochem Grade 500 Zinc Oxide data sheet
Their recommend grade for ceramics. This grade is also widely used in tire and rubber, paint and coatings.
URLs https://www.zochem.com/
Zochem web site
Producer of Zinc Oxide powder with large North American capacity. Their website is for customers and users rather than for investors. They are very open and free with product information and serious about and highly focussed on zinc oxide only.
URLs https://www.zochem.com/products/recommended-products-by-application/
Zochem Zinc Oxide Recommended Products by Application
Click on the grade number in column 1 for its datasheet. These products are used in plastic, rubber, food contact, adhesives, oil and lubrication additives, nutrients, varistors, ferrites.
Materials Zinc Oxide
A pure source of ZnO for ceramic glazes, it is 100% pure with no LOI.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy