| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| ZnO | 51.30% | 1.00 | |
| Al2O3 | 14.50% | 0.23 | |
| SiO2 | 34.20% | 0.90 | |
| Oxide Weight | 158.67 | ||
| Formula Weight | 158.67 | ||
| Materials |
Eutectics
|
| Typecodes |
Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries. |
| Frit Softening Point | 1360C |
|---|