Zeolite

Notes

Natural volcanic silicate mineral having a unique interconnecting lattice structure. It has a honeycomb framework of consistent-diameter interconnecting channels and pores coupled with negatively charged alumina and neutrally charged silica tetrahedra. This produces an open three-dimensional honeycomb framework that attracts liquids, odors & gases and traps them in its crystaline structure. Thus Zeolites are commonly used in environmental cleanup because of their ability to absorb selected pollutants and lock them inside its structure.

Related Information


This picture has its own page with more detail, click here to see it.

Zeolite


This picture has its own page with more detail, click here to see it.

Zeolite Stellerite Crystals

Links

Oxide Analysis Formula Tolerance
URLs http://www.iza-online.org/
International Zeolites Association
Hazards Toxicological Assessment of Zeolites
Abstract from an article from the Journal of the American College of Toxicology 1992

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy