Yellow Ochre

Alternate Names: Hydrated ferric oxide

Description: High iron clay

Oxide Analysis Formula Tolerance
CaO 0.23% 0.02
MgO 0.06% 0.01
Al2O3 19.92% 1.00
SiO2 57.78% 4.92
Fe2O3 22.01% 0.70
Oxide Weight 512.05
Formula Weight 512.05

Notes

A natural clay material containing yellow iron oxide, a hydrated ferric oxide, FeO(OH). Properties will vary in different areas. For many industries, this material is an inexpensive pigment (e.g. for staining cement and mortar). But for ceramics (e.g. as a colorant to produce iron tan, yellow and red-brown in slips and glazes), its iron content determines how useful it is compared to true iron oxide.

Material we have tested has low plasticity. Strangely, yellow iron can be even more plastic than yellow ochre, much stickier when wet.

Related Information

Yellow iron oxide vs. Yellow Ochre - fired at cone 6


yellow iron oxide and yellow ochre

This picture has its own page with more detail, click here to see it.

The rear two samples are just dried. The fired iron oxide (front left) is clearly exhibiting a metallic sheen and has shrunk and become much more dense. And heavy. In the raw state, both exhibit a measure of plasticity when water is added. The yellow iron really holds on to the water, drying out much more slowly. The iron oxide densifies and shrinks even more by cone 8, taking on the characteristics of the metal.

Yellow ochre slurry color


This picture has its own page with more detail, click here to see it.

Just been poured on to a plaster table. It has low plasticity and dewaters quickly.

Yellow Ochre as a low fire body colorant


This picture has its own page with more detail, click here to see it.

It is bright yellow in the raw state, but it still fires red. 10% Yellow Ochre was added to a buff burning stoneware clay. Left is the dried clay. The center sample was fired to 1500F. The right sample was fired to 1850F.

The original container of a bag of Yellow Ochre


This picture has its own page with more detail, click here to see it.

From Davis Colors

Links

Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.
URLs https://www.nrochre.com/products/natural-iron-oxide-pigments
About natural iron oxide pigments: Ochre and Umber
Ochre (pronounced o’-ker) is a natural, mineral, earth pigment. Chemically, it is a hydrated ferric oxide, chemical formulation: FeO(OH). Ochre is inorganic, chemically inert, non-reactive with cement, mortar or brick, and non-toxic.
Materials Iron Oxide Yellow

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy