1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Willemite

Description: Zinc silicate

Formula: Zn2SiO4

Oxide Analysis Formula Tolerance
ZnO 72.98% 1.00
SiO2 27.04% 0.50
Oxide Weight 111.56
Formula Weight 111.56

Related Information

Links

Minerals Willemite
A ore of zinc.

Mechanisms

Glaze CrystallizationSmall zinc silicate crystals can be used to control where crystals grow in crystalline glazes.