1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Vancide MZ-98

Alternate Names: VAncide TH, Vancide 51Z

Description: Bacteria and fungi control agent

Notes

In ceramics, Vancide preservative is used to prevent glazes and slip from deteriorating due to bacteria and fungi (more likely to occur when they contain organic additives). It is a creamy-white powder that is readily dispersible in ceramic glazes and slips.

Zinc dimethyldithiocarbamate Bis(dimethyldithiocarbamoto‐S,S’)zinc
Made by Eastman chemical.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Tektamer 38 Biocide
Materials Dowicil Preservative
Typecodes Biocide
These are added to glazes and bodies to prevent the growth of micro organisms. Often targeted at bacteria, mold or fungi.
URLs https://www.eastman.com/Literature_Center/T/TAM10088.pdf
Ziram fungicide home page
URLs https://www.vanderbiltminerals.com/assets/uploads/documents/technical/TDS_VANCIDE_MZ-98_Web.pdf
Vancide MZ-98 data sheet

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy