1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Uranium Oxide

Alternate Names: Yellowcake, Triuranium Octaoxide, uranium dioxide

Formula: U3O8

Oxide Analysis Formula Tolerance
U3O8 100.00% 1.00
Oxide Weight 842.00
Formula Weight 842.00

Notes

U3O8 is not actually uranium oxide (or uranium dioxide), it is triuranium octoxide. But the title "uranium oxide" is used here to make this page more searchable. U3O8 is the most stable form of uranium and the one to which UO2 found in nature naturally oxidizes to. Very bright reds and yellows can be made using this material. The pages at Wikipedia, referenced below, especially on uranium dioxide, have information on hazards when used in ceramic glazes (a practice common before 1958). It seems logical that during firing U3O8 would be reduced to the more dangerous UO2.

Here is a comment we got from a potter:

"I experimented with uranium in the late 1970s. I bought some at a pottery supply company in the Fraser Valley, B.C. It was a coarse black powdery substance said to be depleted. I made a few glaze tests with it. Then I decided to take the glaze tests which had less than 10% of whatever this black powder was, and the bag of the substance I had bought, to the Simon Fraser University radiation lab.

A researcher talked to me.

He held a test instrument up to the glaze test tiles, and to the bag. Without saying anything more he quickly put the test tiles and the bag into plastic, sealed it, and picked it up with tongs and put it behind a lead wall. Then he pointed out that he loved being around radioactive substances so much he worked full-time with them. But because he was so familiar with radiation, he said, he had learned to be cautious. He said he would never carry a bag emitting as much radiation as the bag I had anywhere near his testicles. (I had walked in with it in my coat pocket). He said even the test glazes had more radiation coming from them than what he would like to have coming from his ceramic dishes. He talked with someone else in the lab, then, looking very dubious, he said I could have my materials back. He didn't think such material should be sold to people who had not studied radiation and how to protect themselves from it. He advised me to make a lead box to keep the material in.

I stopped experimenting with this material. "

Related Information

The uranium oxide crystalline glazes of William Melmstrom


This picture has its own page with more detail, click here to see it.

A screenshot of a page at William Melmstrom's website handspiral.com (he is in Austin, Texas). He is using uranium oxide to make incredible yellow crystalline glazes. The information is here is very educational and enlightening. And the vases he makes: Wow!

Links

URLs http://en.wikipedia.org/wiki/Triuranium_octaoxide
Triuranium Octaoxide at Wikipedia
URLs http://www.handspiral.com/Uranium.htm
Uranium oxide in crystalline glazes by William Melstrom
URLs https://en.wikipedia.org/wiki/Uranium_dioxide
Uranium Dioxide at Wikipedia
Uranium dioxide or uranium(IV) oxide (UO2), also known as urania or uranous oxide, is an oxide of uranium, and is a black, radioactive, crystalline powder that naturally occurs in the mineral uraninite...
Oxides U3O8 - Uranium Oxide
Hazards Uranium and Ceramics
Materials Uranyl Nitrate

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy