Tricalcium Phosphate, F.C.C.

Oxide Analysis Formula Tolerance
CaO 51.00% 0.75 3.0
P2O5 42.00% 0.25 1.5
LOI 7.50%n/a
Oxide Weight 77.17
Formula Weight 85.27

Notes

Various brands contain:
Arsenic: 1-3 ppm
Fluoride: 30-750 ppm
Heavy metals: 10-150ppm

Related Information

Links

Materials Tricalcium Phosphate

Data

Sieve Analysis Dry on 100 mesh: 1.0% max on 200 mesh: 6.0% max
pH for dry powder 5.9-7.1