Oxide Analysis Formula Tolerance
Al2O3 100.00% 1.00
Oxide Weight 102.00
Formula Weight 102.00

Notes

Tabular alumina is made by holding calcined alumina powder just below its 2040C fusion temperature to recrystallize the normally flat crystals into hexagonal, elongated tablet-shaped ones up to 400 microns in size. It is possible to convert near 100% of the crystals and achieve a high chemical purity. The new crystals maintain the same hardness and density and have much better thermal shock resistance.

Tabular aluminas are useful in ceramics, electrical insulators, dielectrics and refractory applications. They are available in sizes from around 40 mesh down to 325 mesh.

Related Information

Where to get Tabular Alumina?


This picture has its own page with more detail, click here to see it.

Online at Ebay.com apparently!

Links

Materials Alumina Hydrate
Materials Alumina
Materials Calcined Alumina
A high-purity Al2O3 used in technical ceramics, refractories, glazes, and bodies for its extreme hardness, high-temperature strength, and chemical stability.
Typecodes Alumina
Alumina products

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy