Description: English kaolin
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 38.00% | 1.00 | |
| SiO2 | 47.00% | 2.10 | |
| Oxide Weight | 228.16 | ||
| Formula Weight | 228.16 | ||
Stockalite is a specially predispersed china clay (it will disperse readily in aqueous media without the need for deflocculant addition).
| Materials |
Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
| By Tony Hansen Follow me on ![]() | ![]() |