1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Stannous Chloride

Alternate Names: Tin(II) chloride

Formula: SnCl2

Oxide Analysis Formula Tolerance
SnO2 79.44% 1.00
Cl 20.56%n/a
Oxide Weight 150.71
Formula Weight 189.72

Notes

This calculation does not have a balanced equation because the material itself does not have oxygen, this has to be taken from the kiln atmosphere during firing.

SnCl2 + O2 -> SnO2 + CL2

Weight of SnCl2 going into kiln: 189.7
Weight of SnO2 out in glaze
(O2 comes from atmosphere during firing): 150.7
2Cl lost during firing: 71
Percentage SnO2 is of original weight going in: 79.44
Remainder is LOI: 20.56

Related Information

Links

URLs http://en.wikipedia.org/wiki/Tin%28II%29_chloride
Stannous Chloride at wikipedia

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy