Stain 6100

Description: Woodland Brown (CrFeZnAlSi)

Notes

Zinc Iron Chromite Brown Spinel, an inorganic pigment, is a reaction product of high temperature calcination in which Zinc (II) Oxide, Iron (II) Oxide, Iron (III) Oxide, and Chromium (III) Oxide in varying amounts are homogeneously and ionically interdiffused to form a crystalline matrix of spinel. Its composition may include any one or a combination of the modifiers Al2O3, NiO, PbO, Sb2O5, SiO2, SnO2, or TiO2.
Old number: 1357

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy