1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Stain 14 M 432

Description: Coral (ZrSiFe)

Notes

Suitable for all glazes especially Zircon opacified types maturing at lower temperatures e.g. wall tiles
Max Firing Temp: 1200C
For Further Information: C47

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.