Stain 14 H 674

Description: Yellow (ZrSiPr)

Notes

Stronger version of 14 H 236
Max Firing Temp: 1300C
For Further Information: C9

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.