Stain 14 H 365

Description: Yellow (ZrV)

Notes

Suitable for all types of glaze especially those maturing at higher temperatures e.g. sanitaryware types - excellent stability
Max Firing Temp: over 1400C
For Further Information: C8

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.