Stain (white)

Description: TIN WHITE OR ZIRCON WHITE

Notes

Some stain companies supply whites intended for adding to stain to lighten them. Use tin white to lighten cobalt blue stains and zircon whites for others.

It is also common to mix stains of lighter color to lighten a darker shade, however this should only be done within stains of the same system. For example, don't try to lighten a chrome-tin pink with a manganese-alumina pink of lighter shade.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy