Stain (green)

Description: Greens (CrCa)

Notes

Color
-----
Bright transparent yellowish green.

Specific Gravity: 3.0-3.5
----------------

Stability/Kiln Atmosphere
-------------------------
Excellent at firing temperatures up to 1200 C with zinc oxide-free glazes having a high content of lime. Stable in moderately reducing conditions.

Compatibility
-------------
Suitable for blending with chrome-cobalt blue-greens to produce bright emerald greens.

Cost
----
Relatively low.

Note: This description is taken from information provided by Blythe Matthey and may or may not apply to stains of this family from other companies.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.
Oxides Cr2O3 - Chrome Oxide

Mechanisms

Glaze ColorRemove any zinc from the host glaze formula, because it turns chromium brown in most situations. Additional calcium may help.