Stain (blue)

Description: Blues (CoAlZn, CoSi)

Notes

Certain colors may employ controlled quantities of calcium or barium compounds as modifiers.

Color Range
-----------
Dark mazarine blue through royal blue to matte blue. Generally darker and more violet in shade than zircon-vandium blues.

Specific Gravity: 3.5-4.5
----------------

Stability/Kiln Atmosphere
-------------------------
Excellent in most types of glazes and bodies for firing in oxidizing or a slightly reducing atmosphere at temperatures over 1450C.

Compatibility
-------------
Suitable for blending with most other types of ceramic colors including zircon-vanadium blues.

Cost
----
Cost is low to moderate, increasing as the cobalt content increases.

Note: This description is taken from information provided by Blythe Matthey and may or may not apply to stains of this family from other companies.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy