Formula: Na2O . SiO2
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 50.70% | 1.00 | |
| SiO2 | 49.30% | 1.00 | |
| Oxide Weight | 122.29 | ||
| Formula Weight | 122.29 | ||
| Glossary |
Eutectic
In ceramics, this term refers to certain chemistries that melt at much-lower-than-expected temperatures. |
| Typecodes |
Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries. |
| Frit Softening Point | 1056C |
|---|