Sodium Fluoride and Lead Fluoride Eutectic

Oxide Analysis Formula Tolerance
NaF 7.80% 1.00
PbF2 92.20% 2.02
Oxide Weight 538.46
Formula Weight 538.46

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 540C