1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Soda-Silica Eutectic 1

Oxide Analysis Formula Tolerance
Na2O 51.50% 1.00
SiO2 48.50% 0.97
Oxide Weight 120.39
Formula Weight 120.39

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 830C