1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Silver Nitrate

Alternate Names: AgNO3

Formula: AgNO3

Oxide Analysis Formula Tolerance
Ag2O 68.22% 1.00
LOI 31.78%n/a
Oxide Weight 231.74
Formula Weight 339.69

Notes

Silver nitrate is highly soluble and forms Ag+ ions when dissolved in water. This ion transfers to ware as adhered material and when fired and reduced the Ag metal gives a gold sheen.

It is possible to dry blend the nitrate and carbonate forms and putting these into a glaze to get a better gold sheen.

100 grams of Carbonate is equivalent to 123 grams Nitrate.

Related Information

Links

Materials Silver Carbonate
Materials Silver Chloride
Materials Silver Phosphate
Hazards Silver Compounds Toxicology
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy