Description: Cuban silica
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 3.70% | 0.94 | |
| MgO | 0.59% | 0.38 | |
| CaO | 1.34% | 0.62 | |
| SiO2 | 85.50% | 36.93 | |
| Fe2O3 | 4.70% | 0.76 | |
| LOI | 4.58% | n/a | |
| Oxide Weight | 2,487.40 | ||
| Formula Weight | 2,606.79 | ||
| Typecodes |
Silica/Quartz
Quartz is very abundant and there are many grades and name brands. |
| By Tony Hansen Follow me on ![]() | ![]() |