Sil-co-sil

Description: Ground Silica

Oxide Analysis Formula Tolerance
CaO 0.01% 0.30
MgO 0.01% 0.42
TiO2 0.04% 0.85
Al2O3 0.06% 1.00
SiO2 99.75%
Fe2O3 0.03% 0.32
LOI 0.10%n/a
Oxide Weight 169,830.00
Formula Weight 170,000.00

Notes

A common brand name of ground silica used in North America. It is used in both glazes and clay bodies.

Mines: OT-Ottawa, IL
P-Pacific, MO
MC-Mill Creek, OK
B-Berkeley Springs, WV
MD-Mapleton Depot, PA

Sieve Analysis:
Name: 250 125 125 125 106 106 106 90 90 90 90
Mine: OT P MC B P OT MC P MD OT B
------------------------------------------------------------
Cum. %, +100 11.0 0.5 0.2 0.5 0.2 0.1 0.1 0.1 0.1 t 0.1
+200 33.0 13.0 9.0 7.5 8.5 7.8 5.4 4.0 4.0 2.7 3.4
+325 47.0 35.0 29.0 26.0 29.0 24.0 22.0 21.0 18.0 16.0 20.0

Grain shape: Rounded
Hardness, Moh: 7.0
Specific Gravity: 2.65
Bulk Density, lbs per cubic foot: 104
Melting Point: 3100F
Theoretical Surface Area, cm2/gm: 138
Actual Surface Area: 162
Coefficient of Area: 1.17
pH: Neutral

Related Information

Links

Typecodes Silica/Quartz
Quartz is very abundant and there are many grades and name brands.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy