1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

SG-328

Alternate Names: SG328

Description: Albany Slip Substitute

Notes

Through years of formulation and reformulation, Karl Miller developed Albany Slip Substitute which is intended to reproduce the physical and performance characteristics of the famed Albany (NY) Slip once mined only two hours from Miller's ceramic lab.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Albany Slip
A pure low plasticity clay that, by itself, melted to a glossy dark brown glaze at cone 10R. It was a popular glaze ingredient for many decades.