Serpentine

Oxide Analysis Formula Tolerance
SiO2 44.00% 0.69
MgO 43.00% 1.00
H2O 13.00%n/a
Oxide Weight 81.54
Formula Weight 93.72

Related Information

Links

Minerals Serpentine
A hydrous magnesium iron phyllosilicate mineral.