1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Raw Sienna

Oxide Analysis Formula Tolerance
Fe2O3 52.00% 2.55
Al2O3 13.00% 1.00
SiO2 23.00% 3.00
H2O 11.60%n/a
Oxide Weight 690.46
Formula Weight 781.07

Related Information

Links

Materials Burnt Sienna
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.