Queenston Shale

Notes

A red burning low plasticity clay mined in Ontario, Canada. It has been used for many years in the brick industry. It is high in soluble salts and matures quickly after cone 02.

Related Information


This picture has its own page with more detail, click here to see it.

Queenston shale fired bars from cone 06 to cone 4. The top two bars are cone 2 and 4, the third from the top is cone 02.

Oxide Analysis Formula Tolerance