Potclays Frit 2281

Description: Lead alumina bisilicate frit

Oxide Analysis Formula Tolerance
SiO2 32.40% 1.85
Al2O3 2.55% 0.09
PbO 65.04% 1.00
Oxide Weight 343.14
Formula Weight 343.14

Notes

No longer listed on their website.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy