Potclays Frit 2273

Description: This is actually Ferro Frit 3134

Oxide Analysis Formula Tolerance
CaO 20.10% 0.68
Na2O 10.30% 0.32
B2O3 23.10% 0.63
SiO2 46.50% 1.48
Oxide Weight 190.69
Formula Weight 190.69

Notes

No longer available from Potclay. They recommend "a 50:50 mix of 2263 and 2268 as the closest alternative" but also recommend that you test beforehand. However such a mix would have 4.5% Na2O, 6% Al2O3, 35% B2O3, 33% SiO2.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3134
A frit with 23% B2O3. The most common of frits used in pottery in North America. Around the world, other companies make frits of equivalent chemistry.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy