Description: This is actually Ferro Frit 3195
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 11.20% | 0.67 | |
| Na2O | 5.99% | 0.33 | |
| Al2O3 | 12.39% | 0.41 | |
| B2O3 | 22.99% | 1.11 | |
| SiO2 | 47.44% | 2.66 | |
| Oxide Weight | 337.58 | ||
| Formula Weight | 337.58 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Materials |
Ferro Frit 3195
A commonly available calcium borosilicate frit. It is glaze-like, needing only a kaolin addition to create a low-temperature semi-glossy glaze. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |