Potclays Frit 2268

Alternate Names: 2268 Kasiumborat fritte, Potclays Calcium Borate Frit

Description: Very high calcium borosilicate frit

Oxide Analysis Formula Tolerance
CaO 27.10% 1.00
Al2O3 4.78% 0.10
B2O3 50.44% 1.50
SiO2 17.68% 0.61
Oxide Weight 207.01
Formula Weight 207.01

Notes

Discontinued 2007

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials PotteryCrafts Frit P2954
A calcium borate frit (with extremely high boron).
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Frit Melting Range (C) 950-1050

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy