1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Potassium Fluoride and Barium Fluoride Eutectic

Oxide Analysis Formula Tolerance
KF 78.70% 1.00
BaF2 21.30% 0.09
Oxide Weight 73.82
Formula Weight 73.82

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 750C