1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pemco Frit Pb-83

Alternate Names: Frit Pb83

Description: Soda-high lead-borosilicate very low melting frit

Oxide Analysis Formula Tolerance
Na2O 6.40% 0.28
PbO 59.20% 0.72
B2O3 14.40% 0.56
SiO2 20.00% 0.90
Oxide Weight 271.40
Formula Weight 271.40

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Ferro Frit 3419
Materials General Frit GF-42
Materials Hommel Frit 33
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 10.4 x 10-6 (50-450C)
Co-efficient of Linear Expansion 10.4 x 10-6 (50-350C)
Frit Melting Range (C) 1000-1050f
I.F.P. (celsius) 453C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy