1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Pemco Frit P-878

Alternate Names: Frit 878, Frit P878

Description: Zirconium opacified frit

Oxide Analysis Formula Tolerance
CaO 14.60% 0.68
Na2O 7.60% 0.32
ZrO2 17.60% 0.37
B2O3 17.00% 0.64
SiO2 43.20% 1.88
Oxide Weight 261.21
Formula Weight 261.21

Notes

Equivalent to 72.7% P-54 and 27.3% zircon.

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.9 x 10-6 (50-450C)
Frit Melting Range (C) 1500-1590F

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://backup.digitalfire.com, All Rights Reserved
Privacy Policy